Current location - Trademark Inquiry Complete Network - Tian Tian Fund - What are the components of Inconel713C high temperature alloy?
What are the components of Inconel713C high temperature alloy?

Overview of Inconel713C/K418/K18/518 equiaxed crystal casting superalloy: Inconel713C is a nickel-based precipitation hardening equiaxed crystal casting superalloy, with γ' phase as the precipitation strengthening phase, and the service temperature is below 900°C.

The alloy has high creep strength, thermal and cold fatigue resistance and oxidation resistance.

The alloy has simple composition, does not contain cobalt, has a low density, and is usually used in the cast state.

Similar brands: Inconel713C or 713C or K418/K18/518Inconel713C Physical properties: Melting point: 1295℃~1345℃; Density: ρ=8.0g/cm3; Expansion coefficient: 20~800℃: 14.7╳10-6℃-1; Room temperature

Hardness (as cast): HRC33~37Inconel713C mechanical properties: 20℃: yield strength 760Mpa, elongation 9.5%; 800℃: yield strength 745Mpa, elongation 9.0%.

Durable high temperature: 800℃, 255Mpa for more than 8000h, 490Mpa for more than 80h.

Main applications and characteristics of Inconel713C: This alloy is suitable for making hot-end rotating and stationary precision castings working below 900°C, such as turbine working blades, guide blades, guides and integrally cast turbines.

It has been widely used in the production of turbine blades, guide vanes and integrally cast turbines for aviation, ground and marine gas turbines, integrally cast turbine rotors and guides for aerospace missile engines, as well as diesel and gasoline engine booster turbines and hot extrusion dies.

The alloy is treated by hot isostatic pressing (HIP) and subsequent heat treatment, which can improve the plasticity and fatigue resistance of the alloy, and can also restore the structure and performance of parts that have experienced structural degradation and reduced performance after long-term use.

When the alloy is used for a long time under hot corrosion conditions, it must have a protective coating.

After long-term aging at 800°C, a small amount of σ phase will precipitate out of the alloy, but it will have no significant impact on its properties.

Main specifications of Inconel713C: Inconel713C round rod has limited space. If you need more detailed introduction, please feel free to inquire.